name='Luigi' said:thanks for that.. What I should have made a bit more clear is that I will be anodizing them with paint, not alu.
name='marcus000' said:lol well thats not anodising them then!
To anodise something you need sulphuric acid, pure distilled water, a power source and colour dyes etc.
I've been toying with the idea of powder coating some barbs glossy black, it might look pretty good.![]()
name='marcus000' said:Shouldn't do no, powder coating doesn't flake like normal paint does, it forms a kind of skin on the object.
I'll try it on some EK barbs and post up the results.![]()
name='marcus000' said:Won't work on compression fittings, it'll knacker the thread right up!![]()
name='PV5150' said:You going to do some anodising yourself luigi? I made a guide quite a while back on doing it if you're interested.
name='marcus000' said:@ Matt
In other guides i've seen people use aluminum wire and aluminum foil to create the cathode, any real difference in doing that and using lead bar?